State of the art of Deep Rolling P Delgado, II Cuesta, JM Alegre, A Díaz Precision Engineering 46, 1-10, 2016 | 127 | 2016 |
The long-term accelerated expansion of various ladle-furnace basic slags and their soil-stabilization applications V Ortega-López, JM Manso, II Cuesta, JJ González Construction and building materials 68, 455-464, 2014 | 116 | 2014 |
Coupled hydrogen diffusion simulation using a heat transfer analogy A Díaz, JM Alegre, II Cuesta International Journal of Mechanical Sciences 115, 360-369, 2016 | 93 | 2016 |
Determination of the Gurson–Tvergaard damage model parameters for simulating small punch tests II Cuesta, JM Alegre, R Lacalle Fatigue & fracture of engineering materials & structures 33 (11), 703-713, 2010 | 88 | 2010 |
Stress-separation techniques in photoelasticity: a review M Solaguren-Beascoa Fernández, JM Alegre Calderón, PM Bravo Diez, ... The Journal of Strain Analysis for Engineering Design 45 (1), 1-17, 2010 | 60 | 2010 |
Determination of the fracture toughness by applying a structural integrity approach to pre-cracked Small Punch Test specimens II Cuesta, JM Alegre Engineering fracture mechanics 78 (2), 289-300, 2011 | 59 | 2011 |
A review on diffusion modelling in hydrogen related failures of metals A Díaz, JM Alegre, II Cuesta Engineering Failure Analysis 66, 577-595, 2016 | 57 | 2016 |
Inverse determination of the elastoplastic and damage parameters on small punch tests I Peñuelas, II Cuesta, C Betegón, C Rodriguez, FJ Belzunce Fatigue & Fracture of Engineering Materials & Structures 32 (11), 872-885, 2009 | 53 | 2009 |
Analysis of different techniques for obtaining pre-cracked/notched small punch test specimens II Cuesta, C Rodriquez, FJ Belzunce, JM Alegre Engineering Failure Analysis 18 (8), 2282-2287, 2011 | 49 | 2011 |
Damage modeling in small punch test specimens E Martínez-Pañeda, II Cuesta, I Peñuelas, A Díaz, JM Alegre Theoretical and applied fracture mechanics 86, 51-60, 2016 | 44 | 2016 |
Effect of HIP post-processing at 850° C/200 MPa in the fatigue behavior of Ti-6Al-4V alloy fabricated by Selective Laser Melting JM Alegre, A Díaz, R García, LB Peral, II Cuesta International Journal of Fatigue 163, 107097, 2022 | 43 | 2022 |
Effect of hydrogen embrittlement on the tensile properties of CrMoV steels by means of the small punch test TE García, C Rodríguez, FJ Belzunce, II Cuesta Materials Science and Engineering: A 664, 165-176, 2016 | 43 | 2016 |
Numerical simulation of hydrogen embrittlement and local triaxiality effects in notched specimens A Díaz, JM Alegre, II Cuesta Theoretical and Applied Fracture Mechanics 90, 294-302, 2017 | 42 | 2017 |
Some aspects about the crack growth FEM simulations under mixed-mode loading JM Alegre, II Cuesta International Journal of Fatigue 32 (7), 1090-1095, 2010 | 42 | 2010 |
Influence of raster orientation on the determination of fracture properties of polypropylene thin components produced by additive manufacturing M Lorenzo-Bañuelos, A Díaz, II Cuesta Theoretical and Applied Fracture Mechanics 107, 102536, 2020 | 40 | 2020 |
Different methodologies to obtain the fracture properties of metallic materials using pre-notched small punch test specimens JM Alegre, R Lacalle, II Cuesta, JA Álvarez Theoretical and applied fracture mechanics 86, 11-18, 2016 | 38 | 2016 |
Hardening evaluation of stamped aluminium alloy components using the small punch test II Cuesta, JM Alegre Engineering Failure Analysis 26, 240-246, 2012 | 38 | 2012 |
Analysis of hydrogen permeation tests considering two different modelling approaches for grain boundary trapping in iron A Díaz, II Cuesta, E Martinez-Pañeda, JM Alegre International Journal of Fracture 223, 17-35, 2020 | 37 | 2020 |
Residual stresses in cold-formed steel members: Review of measurement methods and numerical modelling A Díaz, II Cuesta, JM Alegre, AMP de Jesus, JM Manso Thin-Walled Structures 159, 107335, 2021 | 36 | 2021 |
Determination of the fracture properties of metallic materials using pre‐cracked small punch tests JM Alegre, II Cuesta, HL Barbachano Fatigue & Fracture of Engineering Materials & Structures 38 (1), 104-112, 2015 | 36 | 2015 |