Zachary D. Harris
Title
Cited by
Cited by
Year
Effects of grain size and deformation temperature on hydrogen-enhanced vacancy formation in Ni alloys
SK Lawrence, Y Yagodzinskyy, H Hänninen, E Korhonen, F Tuomisto, ...
Acta Materialia 128, 218-226, 2017
422017
Elucidating the contribution of mobile hydrogen-deformation interactions to hydrogen-induced intergranular cracking in polycrystalline nickel
ZD Harris, SK Lawrence, DL Medlin, G Guetard, JT Burns, BP Somerday
Acta Materialia 158, 180-192, 2018
392018
The Effect of Microstructural Variation on the Hydrogen Environment-Assisted Cracking of Monel K-500
ZD Harris, JD Dolph, GL Pioszak, BCR Troconis, JR Scully, JT Burns
Metallurgical and Materials Transactions A 47 (7), 3488-3510, 2016
252016
On the suitability of slow strain rate tensile testing for assessing hydrogen embrittlement susceptibility
E Martínez-Pañeda, ZD Harris, S Fuentes-Alonso, JR Scully, JT Burns
Corrosion Science 163, 108291, 2020
242020
Measurement and modeling of hydrogen environment-assisted cracking in a Ni-Cu-Al-Ti superalloy
JT Burns, ZD Harris, JD Dolph, RP Gangloff
Metallurgical and Materials Transactions A 47 (3), 990-997, 2016
222016
The effect of heat-to-heat variations in metallurgy and hydrogen-metal interactions on the hydrogen embrittlement of Monel K-500
BCR Troconis, ZD Harris, H Ha, JT Burns, JR Scully
Materials Science and Engineering: A 703, 533-550, 2017
162017
The effect of electrode potential on stress corrosion cracking in highly sensitized Al–Mg alloys
ME McMahon, ZD Harris, JR Scully, JT Burns
Materials Science and Engineering: A 767, 138399, 2019
82019
The effect of isothermal heat treatment on hydrogen environment-assisted cracking susceptibility in Monel K-500
ZD Harris, JT Burns
Materials Science and Engineering: A 764, 138249, 2019
72019
The combined effects of hydrogen and aging condition on the deformation and fracture behavior of a precipitation-hardened nickel-base superalloy
ZD Harris, JJ Bhattacharyya, JA Ronevich, SR Agnew, JT Burns
Acta Materialia 186, 616-630, 2020
62020
Examination of focused ion beam-induced damage during platinum deposition in the near-surface region of an aerospace aluminum alloy
AW Thompson, ZD Harris, JT Burns
Micron 118, 43-49, 2019
62019
Multiscale Assessment of Deformation Induced by Hydrogen Environment-Assisted Cracking in a Peak-Aged Ni-Cu Superalloy
ZD Harris, AW Thompson, JT Burns
JOM, 1-10, 2020
32020
Elucidating the loading rate dependence of hydrogen environment-assisted cracking in a Ni-Cu superalloy
ZD Harris, EM Dubas, AS Popernack, BP Somerday, JT Burns
Theoretical and Applied Fracture Mechanics 111, 102846, 2021
12021
Assessing the fatigue crack growth behavior of highly sensitized AA5456-H116 under cathodic polarization
ZD Harris, EM Dubas, DJ Schrock, JSW Locke, JT Burns
Materials Science and Engineering: A 792, 139792, 2020
12020
On the hydrogen environment-assisted cracking resistance of a compositionally complex Co–Ni–Cr–Fe–Mo–Ti alloy
ZD Harris, K Guiseva, JR Scully, JT Burns
Materials Science and Engineering: A 802, 140601, 2021
2021
Assessing the influence of hydrogen on texture evolution in polycrystalline nickel deformed under uniaxial tension
ZD Harris, MA Ritzo, JM Schulte, SR Agnew, JT Burns
Scripta Materialia 188, 238-243, 2020
2020
On the fatigue crack growth behavior of Ti–10V–2Fe–3Al in gaseous hydrogen
ZD Harris, JA Ronevich, V Stavila, BP Somerday
International Journal of Hydrogen Energy 45 (51), 27929-27940, 2020
2020
The Effect of Heat Treatment on Hydrogen Environment-Assisted Cracking of Monel K-500
ZD Harris, JT Burns
International Hydrogen Conference (IHC 2016): Materials Performance in …, 2017
2017
The Influence of Deformation Temperature on the Initiation of Hydrogen-Induced Intergranular Cracking in Nickel
ZD Harris, SK Lawrence, G Guetard, JT Burns, BP Somerday
International Hydrogen Conference (IHC 2016): Materials Performance in …, 2017
2017
The system can't perform the operation now. Try again later.