Fabrication of ZrO2–NiCr functionally graded material by powder metallurgy J Zhu, Z Lai, Z Yin, J Jeon, S Lee Materials chemistry and physics 68 (1-3), 130-135, 2001 | 389 | 2001 |
Effect of SrTiO3 concentration and sintering temperature on microstructure and dielectric constant of Ba1− xSrxTiO3 JH Jeon Journal of the European Ceramic Society 24 (6), 1045-1048, 2004 | 186 | 2004 |
Microstructure and dielectric properties of barium–strontium titanate with a functionally graded structure JH Jeon, YD Hahn, HD Kim Journal of the European Ceramic Society 21 (10-11), 1653-1656, 2001 | 85 | 2001 |
(K,Na)NbO3‐Based Ceramics for Piezoelectric “Hard”Lead‐Free Materials JB Lim, S Zhang, JH Jeon, TR Shrout Journal of the American Ceramic Society 93 (5), 1218-1220, 2010 | 73 | 2010 |
pH control of magnetic properties in precipitation-hydrothermal-derived CoFe2O4 S Jovanović, M Spreitzer, M Otoničar, JH Jeon, D Suvorov Journal of alloys and compounds 589, 271-277, 2014 | 46 | 2014 |
A Si-Mo fused slurry coating for oxidation protection of carbon-carbon composites HT Fang, JC Zhu, ZD Yin, JH Jeon, YD Hahn Journal of materials science letters 20, 175-177, 2001 | 43 | 2001 |
Effect of Al additive in Si slurry coating on liquid Si infiltration into carbon–carbon composites HT Fang, ZD Yin, JC Zhu, JH Jeon, YD Hahn Carbon 39 (13), 2035-2041, 2001 | 40 | 2001 |
Inhibition of liquid Si infiltration into carbon–carbon composites by the addition of Al to the Si slurry pre-coating: mechanism analysis HT Fang, JH Jeon, JC Zhu, ZD Yin Carbon 40 (14), 2559-2565, 2002 | 30 | 2002 |
Recrystallization in cast 45-2-2 XD™ titanium aluminide during hot isostatic pressing JH Jeon, AB Godfrey, PA Blenkinsop, W Voice, YD Hahn Materials Science and Engineering: A 271 (1-2), 128-133, 1999 | 28 | 1999 |
Shear‐Mode Piezoelectric Properties of Modified‐(K,Na)NbO3 Ceramics for “Hard” Lead‐Free Materials JB Lim, S Zhang, HJ Lee, JH Jeon, TR Shrout Journal of the American Ceramic Society 93 (9), 2519-2521, 2010 | 24 | 2010 |
Microstructural development of cobalt ferrite ceramics and its influence on magnetic properties GY Kim, JH Jeon, MH Kim, D Suvorov, SY Choi Metals and Materials International 19, 1209-1213, 2013 | 21 | 2013 |
Effect of Sintering Atmosphere on Interface Migration of Niobium‐Doped Strontium Titanate during Infiltration of Oxide Melts JH Jeon, SJL Kang Journal of the American Ceramic Society 77 (6), 1688-1690, 1994 | 20 | 1994 |
Mechanism of Bi0. 5Na0. 5TiO3 and Bi4. 5Na0. 5Ti4O15 template synthesis during topochemical microcrystal conversion and texturing of Bi0. 5 (Na0. 8K0. 2) 0.5 TiO3 piezoelectric … HA Cha, YK Kim, JH Jeon Journal of the European Ceramic Society 37 (3), 967-974, 2017 | 18 | 2017 |
Manufacture of a micro-sized piezoelectric ceramic structure using a sacrificial polymer mold insert JH Kim, SY Choi, JH Jeon, G Lim, SS Chang Microsystem technologies 19, 343-349, 2013 | 18 | 2013 |
Phase constitutions of MoSiN anti-oxidation multi-layer coatings on CC composites by fused slurry ZH Lai, JC Zhu, JH Jeon, B Zhang, J Yu Materials Science and Engineering: A 499 (1-2), 267-270, 2009 | 16 | 2009 |
Control of Interface Migration in Melt‐Infiltrated Niobium‐Doped Strontium Titanate by Solute Species and Atmosphere JH Jeon, JH Je, SJL Kang Journal of the American Ceramic Society 81 (3), 624-628, 1998 | 15 | 1998 |
Optimisation of matrix composition for texturing of morphotropic phase boundary Pb (Mg1/3Nb2/3) O3–PbZrO3–PbTiO3 piezoelectric ceramics using BaTiO3 template M Kim, A Upadhyay, KW Lim, TT Zate, JH Jeon Journal of the European Ceramic Society 41 (15), 7639-7644, 2021 | 14 | 2021 |
Influence of TEM specimen preparation on chemical composition of Pb (Mg1/3Nb2/3) O3–PbTiO3 single crystals V Srot, M Gec, PA van Aken, JH Jeon, M Čeh Micron 62, 37-42, 2014 | 13 | 2014 |
Mechanochemical synthesis and mechanochemical activation-assisted synthesis of alkaline niobate-based lead-free piezoceramic powders JH Jeon Current Opinion in Chemical Engineering 3, 30-35, 2014 | 13 | 2014 |
Piezoelectric and ferroelectric properties of textured (Na0.50K0.47Li0.03)(Nb0.8Ta0.2)O3 ceramics by using template grain growth method HJ Cho, MH Kim, TK Song, JS Lee, JH Jeon Journal of Electroceramics 30, 72-76, 2013 | 12 | 2013 |